eSUN

PET

PET1.75 mm

Print parameters

Diameter1.75 mm
Nozzle250–280 °C
Bed70–90 °C
Speed≤ 250 mm/s
Fan40–70 %
Drying (temp / time)—
Density1.28 g/cm³
Mechanical & thermal properties
Tensile strength–/40XY/ZMPa
Tensile modulus–MPa
Elongation at break–/5XY/Z%
Flexural strength95/–XY/ZMPa
Impact strength4/–XY/ZkJ/m²
Hardness—
HDT (heat deflection)70°C
Glass transition (Tg)—
VICAT–°C
Verified against manufacturer datasheet

This data comes from the manufacturer's technical sheets and website. FilamentCat only displays it — I don't guarantee it; verify with the manufacturer before printing. Values may vary by printer and conditions.