Forward AM

Ultrafuse TPU 64D

TPU1.75 mm

Print parameters

Diameter1.75 mm
Nozzle230–255 °C
Bed40–60 °C
Speed30–60 mm/s
Fan—
Drying (temp / time)70 °C / 5 h
Density1.157 g/cm³
Mechanical & thermal properties
Tensile strength37MPa
Tensile modulus205MPa
Elongation at break399%
Flexural strength–MPa
Impact strength115kJ/m²
Hardness58 Shore D Shore
HDT (heat deflection)–°C
Glass transition (Tg)-26 °C
VICAT–°C
Data from manufacturer's website

This data comes from the manufacturer's technical sheets and website. FilamentCat only displays it — I don't guarantee it; verify with the manufacturer before printing. Values may vary by printer and conditions.