CR-3D
PP FibCR20
PP-GF
Requires hardened nozzle
Print parameters
| Nozzle | 250 °C |
|---|---|
| Bed | 50 °C |
| Speed | — |
| Fan | — |
| Drying (temp / time) | — |
| Density | 0.98 g/cm³ |
Mechanical & thermal properties
| Tensile strength | 105MPa |
|---|---|
| Tensile modulus | 2564MPa |
| Elongation at break | 5% |
| Flexural strength | –MPa |
| Impact strength | 14.45kJ/m² |
| Hardness | — |
| HDT (heat deflection) | 125°C |
| Glass transition (Tg) | — |
| VICAT | –°C |
Data from manufacturer's website
This data comes from the manufacturer's technical sheets and website. FilamentCat only displays it — I don't guarantee it; verify with the manufacturer before printing. Values may vary by printer and conditions.