Forward AM
Ultrafuse ABS
ABS
Requires enclosure
Print parameters
| Nozzle | 240–260 °C |
|---|---|
| Bed | 90–110 °C |
| Speed | 40–80 mm/s |
| Fan | — |
| Drying (temp / time) | 60 °C / 10 h |
| Density | 1.037 g/cm³ |
Mechanical & thermal properties
| Tensile strength | 36.3MPa |
|---|---|
| Tensile modulus | 1958MPa |
| Elongation at break | 7.4% |
| Flexural strength | 56.6MPa |
| Impact strength | 16kJ/m² |
| Hardness | D71 Shore |
| HDT (heat deflection) | 90°C |
| Glass transition (Tg) | 104 °C |
| VICAT | 96°C |
Data from manufacturer's website
This data comes from the manufacturer's technical sheets and website. FilamentCat only displays it — I don't guarantee it; verify with the manufacturer before printing. Values may vary by printer and conditions.