Forward AM
Ultrafuse BVOH
BVOH
Print parameters
| Nozzle | 190–210 °C |
|---|---|
| Bed | 60–100 °C |
| Speed | 30–60 mm/s |
| Fan | — |
| Drying (temp / time) | 60 °C / 16 h |
| Density | 1.138 g/cm³ |
Mechanical & thermal properties
| Tensile strength | 33.7MPa |
|---|---|
| Tensile modulus | 2339MPa |
| Elongation at break | 14.8% |
| Flexural strength | 53.8MPa |
| Impact strength | –kJ/m² |
| Hardness | — |
| HDT (heat deflection) | –°C |
| Glass transition (Tg) | 69 °C |
| VICAT | –°C |
Data from manufacturer's website
This data comes from the manufacturer's technical sheets and website. FilamentCat only displays it — I don't guarantee it; verify with the manufacturer before printing. Values may vary by printer and conditions.