Print parameters
| Nozzle | 260–280 °C |
|---|---|
| Bed | 70–90 °C |
| Speed | 10–30 mm/s |
| Fan | — |
| Drying (temp / time) | — |
| Density | 1.044 g/cm³ |
Mechanical & thermal properties
| Tensile strength | 7MPa |
|---|---|
| Tensile modulus | 54MPa |
| Elongation at break | 280% |
| Flexural strength | –MPa |
| Impact strength | 14.1kJ/m² |
| Hardness | 89A Shore |
| HDT (heat deflection) | –°C |
| Glass transition (Tg) | -59 °C |
| VICAT | –°C |