Forward AM

Ultrafuse TPU 85A

TPU

Print parameters

Nozzle200220 °C
Bed40 °C
Speed1540 mm/s
Fan
Drying (temp / time)70 °C / 5 h
Density1.114 g/cm³
Mechanical & thermal properties
Tensile strength34MPa
Tensile modulus20MPa
Elongation at break600%
Flexural strengthMPa
Impact strengthkJ/m²
Hardness85A Shore
HDT (heat deflection)°C
Glass transition (Tg)-44 °C
VICAT35°C
Data from manufacturer's website

This data comes from the manufacturer's technical sheets and website. FilamentCat only displays it — I don't guarantee it; verify with the manufacturer before printing. Values may vary by printer and conditions.