Forward AM

Ultrafuse TPU 95A

TPU

Print parameters

Nozzle210230 °C
Bed40 °C
Speed1540 mm/s
Fan
Drying (temp / time)70 °C / 5 h
Density1.149 g/cm³
Mechanical & thermal properties
Tensile strength44.2MPa
Tensile modulus48.4MPa
Elongation at break661%
Flexural strengthMPa
Impact strengthkJ/m²
Hardness92A Shore
HDT (heat deflection)°C
Glass transition (Tg)-25 °C
VICAT75°C
Data from manufacturer's website

This data comes from the manufacturer's technical sheets and website. FilamentCat only displays it — I don't guarantee it; verify with the manufacturer before printing. Values may vary by printer and conditions.