Sunlu

TPU 95A

TPU

Print parameters

Nozzle200230 °C
Bed2560 °C
Speed3060 mm/s
Fan
Drying (temp / time)50 °C /
Density1.23 g/cm³
Mechanical & thermal properties
Tensile strength34.4/XY/ZMPa
Tensile modulus50.2MPa
Elongation at break1063%
Flexural strength4.26MPa
Impact strengthkJ/m²
Hardness95HA Shore
HDT (heat deflection)52°C
Glass transition (Tg)
VICAT°C
Data from manufacturer's website